Catalyst
Specific Type |
|
ITEM |
UNITS |
ZnO For Desulfurizer |
Type NC for dechlorinating |
PIA Catalyst |
HCL-200 dechlorinating |
Active component and content |
% |
Zn0.96% |
- |
KMnO4-Al2O3 |
|
Activated alumina |
% |
- |
- |
≥80 |
|
Potassium permanganate |
% |
- |
- |
5±0.5 |
|
Fe2O3 |
wt% |
|
|
|
≤0.1 |
Alumina +Accelerant |
wt% |
|
|
|
≥95.5,OR≥99.7 |
Appearance and Color |
|
Light yellow strip |
Grey spherical |
Purple or pink spherical |
White spherical |
Apparent and Sizes(mm) |
mm |
Solid4*4-10 |
3~5 |
4~5、5~7 |
3~5 |
Bet surface |
m2/g |
≥30 |
- |
≥150 |
≥260 |
Pore Diameter |
ml/g |
≥0.4 |
- |
- |
≥0.42 |
Bulk density |
|
1.1-1.3kg/L |
0.78±0.03g/cm3 |
0.8±0.15g/ml |
0.7~0.85g/cm3 |
Crush strength |
|
40N/cm |
≥30N/Grain |
≥40N |
≥120N/Grain |
ATTRITION |
% |
≤5 |
≤1 |
- |
|
Saturated sulfur let |
% |
≥30 |
- |
- |
|
Through sulfur let |
% |
≥20(220℃) ≥30(360℃) |
- |
- |
|
Use Temperature |
℃ |
220-400℃ |
5-100℃ |
- |
|
Use Pressure,MPa |
MPa |
Normal pressures-4.0 |
Normal pressures-10.0 |
- |
|
Feed Gas/Steam |
|
1-1.5:1 |
- |
- |
|
Air-Carrying(h-1)Gas and Liquid |
|
1000-3000 1-6(Liquid) |
- |
- |
|
Purification degrees |
ppm |
- |
<0.5 |
- |
|
Dynamic chlorine content |
% |
- |
≥25(Gaseous state) |
- |
|
Absorb chlorine content |
wt% |
|
|
|
≥10 |
H2S(ppm) under Feeding |
ppm |
≤100 |
- |
- |
|
H2S(PPM) under Discharging |
ppm |
0.1 |
- |
- |
|
1000°C Loss on ignition |
wt% |
|
|
|
≤7.0 |
moisture (100°CDrying to constant weight) |
% |
- |
- |
≤20 |
|
|